stockyard venues and carriageways must be ground treatment and surface hardening, and meet the requirements of heavy vehicles; site should drainage facilities, drainage flow, no significant accumulation of water or crater phenomena. Site field view.
2013年8月12日星期一
unburned aerated block production line ingredients, mixing, pouring
Concrete mixing plant, mixing, pouring lime, cement powder batching position by the screw conveyor under the automatic measurement scale in order to accumulate measurement scales under the screw conveyor can be added to the material evenly pouring blender. Fly ash (or sand, stone powder) and waste slurry into the measuring vat measured in a variety of concrete block making machine in place after the mold case, you can make the slurry stirred before pouring the slurry should meet process requirements (approximately 45 ℃), if the temperature is not
enough, can be measured in a slurry tank through steam heating in the materials before pouring 0.5 to 1 minute to join aluminum suspension.